相变材料(PCM)凭借其高潜热与近等温储放热特性,在热能储存与热管理领域展现出巨大潜力。然而,熔融泄漏、本征热导率低以及固态刚性等问题,阻碍了其在高储能密度下同时实现尺寸稳定性、柔性、界面自适应性与多功能响应。因此,开发兼顾高储能与超柔性的复合相变材料具有重要意义。基于此,本文,南昌大学胡小武教授团队在《Advanced Functional Materials》期刊发表名为”Static–Dynamic Hybrid Covalent Networks Enable Scale-Selective Molecular Confinement in Ultraflexible Phase Change Composites for Adaptive Thermal Management”的论文,研究提出了一种静态-动态杂化共价三维网络结合石墨烯纳米片(GNPs)快速导热通道的策略。该石蜡基复合相变材料(CPCM)以静态共价键维持网络完整性,以可交换硼酸酯键实现热触发重排,从而对石蜡实施尺度选择性分子限域。
此外,实验与模拟结果共同证明,该交联网络在抑制石蜡大尺度协同迁移的同时,保留了可逆相变所需的局部自由度,从根本上化解了”防泄漏”与”相变失效”之间的矛盾。经测试,该 CPCM 相变焓达 172.2 J/g,断裂伸长率高达 1219.5%;引入 GNP 后热导率提升至 2.07 W/m·K,且焓效率仍保持在 98.8% 以上;同时兼具优异的粘附性、自修复、可回收与形状记忆性能,使其适用于电子器件热管理、宽温域电池、太阳能储热与柔性可穿戴热管理。本研究提出了一种静态-动态杂化共价网络设计策略,该策略显著增强了相变材料的超柔性、结构稳定性与动态界面适应性,并为在单一相变材料体系中集成高储能、超柔性与多功能响应提供了新的设计路线。

图1、The preparation process, application scenarios, and comprehensive performance of CPCM, a hybrid static-dynamic covalent three-dimensional network. (a) Fabrication process and schematic diagram of the network structure of CPCM. (b) Schematic illustration of CPCM applications in multiple application scenarios. (c) DSC curves and high latent-heat energy storage performance of G7 and G9 samples. (d) Characterization demonstration of the film-forming capability, ultra-flexibility, and load-bearing adhesion performance of CPCM. (e) A radar chart comparing the comprehensive advantages of this work with those of different types of flexible phase-change materials. Quantitative indicators including flexibility, latent heat, self-healing efficiency, and adhesive strength are evaluated based on fracture strain, melting enthalpy, strength recovery rate, and experimentally measured adhesive strength, respectively. All indicators are normalized against the maximum value reported in the comparison system. Shape stability and shape memory effect are evaluated based on whether the existence of these properties has been experimentally verified in relevant studies.
本文提出一种静态-动态杂化共价网络结合 GNP 导热通道的设计策略:静态共价键维持网络完整性,可交换硼酸酯键赋予热触发重排能力,对石蜡实现尺度选择性分子限域——既抑制大尺度协同迁移防泄漏,又保留局部自由度保障可逆相变。所得 CPCM 相变焓 172.2 J/g、断裂伸长率 1219.5%,引入 GNP 后热导率达 2.07 W/m·K 而焓效率仍 >98.8%,并兼具粘附、自修复、可回收与形状记忆性能,在电子热管理、宽温域电池、太阳能储热与可穿戴热管理中表现优异。因此,本研究有望为高储能、超柔性、结构稳定与动态界面自适应一体化的相变材料体系提供新的设计思路。
文献:https://doi.org/10.1002/adfm.79642
本文来自材料分析与应用,本文观点不代表石墨烯网立场,转载请联系原作者。